The process starts by heating lithium and the transition metal of choice, such as cobalt, to 700–1,000 °C to form an oxide powder. The high-temperature process ensures the oxide has good crystallinity, which is necessary for high performance. The resulting powder then gets blended with binders and other additives to make an electrode.